TROUBLESHOOTING / SINK MARKS

Sink marks point to local shrinkage or a packing problem.

A visible depression usually appears where a thick section, rib, boss or local hot area continues to shrink after the surface freezes. The right fix depends on whether the cause is part design, cooling, gating, packing or process instability.

ABERY engineering note
Updated November 20, 2026

Do not automatically increase packing pressure. First identify the local heat and volume demand behind the surface.

QUICK ANSWER

Check the thick-section geometry, rib and boss thickness, gate and runner configuration, local cooling and gate freeze. Then review packing, hold time, melt and mold temperature and cycle stability. Correct the dominant volume-shrinkage source and verify appearance across cavities.

1. Locate the sink and its local geometry.

A sink mark is not uniformly distributed across a part. It often appears over a rib, boss, thick wall, gate area or transition where the local mass stays molten longer. Record the location, depth, lighting condition and cavity number.

Compare the visible depression with the opposite surface and the local wall thickness. A small surface mark can indicate a larger internal void or dimensional issue.

  • Photograph under controlled lighting.
  • Measure or section the local wall thickness.
  • Record cavity, gate and flow direction.
  • Check whether the mark follows one cavity or all cavities.
  • Compare the defect before and after packing changes.

2. Review cooling and gate freeze.

Thick sections and hot cores can remain molten after the surrounding surface has frozen. If the gate freezes before the local section receives enough packing, a sink can form even when the overall packing pressure appears high.

A hot spot may require a baffle, bubbler, insert or local cooling change. The process should be verified with a gate-freeze and cavity-pressure review where available.

Rib or bossCheck thickness ratio, radius and local cooling.
GateCheck gate size, location, freeze time and pressure transfer.
CoolingCheck water flow, circuit balance and hot spots.
PackingReview pressure, hold time and transfer point.
MaterialCheck grade, shrinkage and drying.
ProcessCheck melt temperature, cycle and recovery stability.

Look for the cause.

A higher packing number may increase stress without fixing a local hot spot.

Review mold design

3. Correct the process with limits.

If the sink is marginal and the gate is still open, optimize packing and hold time while monitoring dimensions and stress. If the gate has already frozen, extending hold time may not deliver more material to the local area.

Higher melt temperature can improve flow but may increase shrinkage, flash or degradation risk. Cooling changes and part-design changes can be more durable than a narrow process workaround.

  • Change packing and hold time in documented steps.
  • Confirm gate freeze and cavity pressure where available.
  • Check if the correction affects warpage or flash.
  • Verify all cavities, not only the visibly affected one.
  • Record the approved process window.

4. When the design should change.

If the local mass cannot be packed or cooled consistently, review rib thickness, boss wall, radius, gating or ejector layout. A design change may be the better production solution.

The decision should be based on the functional requirement and the customer’s approval path. Do not machine steel until the root cause and correction are agreed.

Send the evidence.

Include the part, material, process sheet, photos and cavity-specific samples.

Discuss a sink-mark issue

Questions buyers ask before approving this scope.

Do sink marks always mean packing pressure is too low?
No. They can come from local thick sections, hot spots, gate freeze, insufficient cooling, material shrinkage or unstable recovery. Packing is only one part of the diagnosis.
Can sink marks be removed by increasing cycle time?
Sometimes longer cooling can help, but it may not correct a gate or local mass issue. The process change should be verified with dimensions and appearance.
Why does one cavity sink while others do not?
Cavity balance, cooling, gate condition, venting, steel temperature or flow-path differences can create a cavity-specific result.
Should a sink mark be measured or visually judged?
Define the appearance standard and inspection lighting. For functional or assembly surfaces, add a dimensional or section requirement where appropriate.

Need a project-specific answer?

Send the part, material, volume and stage. We will identify what can be confirmed before quotation or tooling.

Send the project

Keep the scope comparable.

The linked guides are written to support a project-specific supplier and tooling review.

PROJECT INTAKE / DEFECT REVIEW

Give the defect a traceable cause.

Send the part photos, material, process sheet and cavity data. We will identify the first review questions and the evidence needed for correction.

Part photosResin gradeProcess sheetCavity numberSample timingMold layout

Tell us where the project is now.

Send the files and context you have. Missing information can be confirmed during review.

A-MOLD Project Inquiry

Business inquiries only. For large files, include a secure Google Drive, Dropbox, OneDrive or WeTransfer link, or email tonney@a-mold.com after submitting.