TROUBLESHOOTING / DEFECT REVIEW
Troubleshoot the system, not the symptom.
Injection molding defects can come from part design, tooling, material, machine, process, measurement or handling. These guides organize the first checks and the evidence needed for a durable correction.
Do not change five process parameters at once. A stable correction must work across cavities and a production run.
START HERE
Classify the defect, record the affected cavities and samples, review the process and material history, then test the highest-confidence cause with a controlled change. Keep the measurement method and sample condition consistent.
Troubleshoot the system, not the symptom.
Warpage troubleshooting
Shrinkage, cooling, fiber orientation, packing and measurement.
Sink-mark troubleshooting
Local mass, gate freeze, cooling and packing.
Weld-line troubleshooting
Flow-front merging, venting, appearance and strength.
Color-streak troubleshooting
Purge, heat history, mixing, material and stress.
Splay and silver streaks
Moisture, gas, shear, venting and heat history.
PROJECT INTAKE / DEFECT REVIEW
Send the defect with a traceable process record.
Include the part, cavity, material, process sheet and samples. We will identify the first review path and missing evidence.
Tell us where the project is now.
Send the files and context you have. Missing information can be confirmed during review.
Business inquiries only. For large files, include a secure Google Drive, Dropbox, OneDrive or WeTransfer link, or email tonney@a-mold.com after submitting.